275 kHz Composites vs. K350 Piezoelectric Ceramic
| ELECTROMECHANICAL PROPERTIES COMPARISON: K350 Ceramic Compared to 275 kHz Composites (three variations using the K350 ceramic) |
|||||||||||||
| Note: The above values are nominal. | |||||||||||||
| Fa | Fa | Fa/Fr | Zr | qr | C | D | kt | K3 | Qm | d33 | nt | ||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Sample | (kHz) | (kHz) | (ohms) | (deg) | (pF) | pm/V | kHz-in | ||||||
| K350 Ceramic | 328 | 313 | 1.048 | 78 | -5 | 1175 | 0.012 | 0.328 | 1825 | 63 | 394 | 78.25 | |
| 275 kHz A | 396 | 277 | 1.42 | 140 | -11 | 593 | 0.017 | 0.739 | 653 | 13.4 | 370 | 55.4 | |
| 275 kHz B | 375 | 277 | 1.35 | 333 | -20 | 565 | 0.019 | 0.689 | 638 | 6.7 | 410 | 55.4 | |
| 275 kHz C | 331 | 273 | 1.21 | 113 | -2 | 559 | 0.015 | 0.604 | 634 | 28.6 | 432 | 54.6 | |
| PHYSICAL PROPERTIES COMPARISON: K350 Ceramic Compared to 275 kHz Composites (three variations using the K350 ceramic) |
|||||
| Note: The above values are nominal. | |||||
| Vol. % Ceramic | qr | Diameter | Thickness | Acoustic Impedance | |
|---|---|---|---|---|---|
| Sample | (%) | (g/cm3) | (in) | (in) | (MRayL) |
| K350 Ceramic | 100 | 7.80 | 0.998 | 0.250 | 31.0 |
| 275 kHz A | 40 | 3.72 | 0.998 | 0.200 | 10.5 |
| 275 kHz B | 40 | 3.78 | 0.998 | 0.200 | 10.6 |
| 275 kHz C | 40 | 3.84 | 0.998 | 0.200 | 10.7 |