Please Note: You are viewing the unstyled version of Piezo Technologies. Either your browser does not support CSS (Cascading Style Sheets) or it is disabled. As a result, much of this website will not look the way it was intended, although all of its contents will be accessible to you. For more information, visit our Browser Support page.

Information Request

Piezo Tech is ISO 9001:2000 Certified. Certification No. C2006-02533. Etalon logo


PIEZOELECTRIC EXAMPLE 2

1.25 MHz Composites vs. K350 Piezoelectric Ceramic

  ELECTROMECHANICAL PROPERTIES COMPARISON:
K350 Ceramic Compared to 2.00 MHz Composites
(three variations using the K350 ceramic)
Note:  The above values are nominal. 
  Fa Fa Fa/Fr Zr qr C D kt K3 Qm d33 nt
Sample (kHz) (kHz)   (ohms) (deg) (pF)         pm/V kHz-in
K350 Ceramic 1.424 1.263 1.127 2.30 4 5578 0.013 0.499 1883 46 435 78.00
2.0 MHz A 2.81 2.08 1.37 10.90 -34 2504 0.034 0.705 410 6.07 420 56.10
2.0 MHz B 2.55 1.92 1.32 8.80 -34 3810 0.045 0.668 646 5.73 390 53.80


  PHYSICAL PROPERTIES COMPARISON:
K350 Ceramic Compared to 2.00 MHz Composites
(three variations using the K350 ceramic)
Note:  The above values are nominal. 
  Vol. % Ceramic qr Diameter Thickness Acoustic Impedance
Sample (%) (g/cm3) (in) (in) (MRayL)
K350 Ceramic 100 7.80 1.00 0.061 30.9
2.0 MHz A 50 4.55 1.00 0.028 13.0
2.0 MHz B 50 4.40 1.00 0.028 12.0


Top of Page